Objectives:

(i) to estimate mineralogical composition specifically clay mineralogy from the spectra,
(ii) to qualitatively compare mineral concentrations calculated from XRF and XRD analyses, as well as mineral groups identified through SEM and microscopic petrography work with NIR results.

NIR spectroscopy has been widely used in different scientific fields such as biology and medicine. However, it has been rarely used in mineral identification in finer sedimentary rocks specifically mudrocks. This work will allow us to verify the accuracy of this technique compared with XRF and XRD.

Login

 
  You need to provide a valid email address which will also be your username for the site.

Not registered yet?

Sign up for free today. By registering you will have free access to exclusive content including

  • Webinars, presentations and videos
  • Application notes, technical notes, articles, white papers and software downloads

And in addition you will receive

  • Our regular eNews including the latest news, education, events and offers from Malvern Panalytical