This application note shows that the Epsilon 4 is capable of analyzing Ni, Co, Mg, Fe, Mn, Zn, Al, Cr, Ca and Si in nickel ore samples.

Accurate elemental analysis of nickel ore samples plays a very important role in nickel ore mine mapping and nickel ore pricing. XRF analysis provides a useful tool for classifying and for the quality control of compositions of the nickel ore materials.