Find out moreThe success of XRF analysis depends on the quality of the calibration standards used. Finding high-quality standards in the required analytical range is not only challenging but also expensive.
WROXI – CRM is a synthetic, high-quality Certified Reference Materials (CRM) kit that covers a wide range of oxide materials such as ores, rocks, and geological materials. It is commonly used in mining, raw materials (cement, steel, metal), slags, service laboratories, R&D facilities, and geological surveys, and has a dual purpose: either for primary fusion glass disk calibration or to develop secondary pressed powder calibrations.
WROXI was developed by our XRF experts to solve the problem of finding suitable calibration material for WD and ED-XRF. It is the solution to the limited availability and elemental ranges of RM/CRMs from natural materials. Being synthetic, WROXI standards will be available forever, and that means there is no risk of the requested CRM being sold out or otherwise unavailable. The kit is shipped with monitors and templates suitable for the Axios-mAX, Zetium and Epsilon 4 spectrometers. The methods and fusion recipes are provided for each Malvern Panalytical fusion instrument. Borate flux and additives, instructions on use, and full SDS are also part of the kit.
WROXI-CRM is manufactured under ISO 17034 accreditation which means the traceability is guaranteed. The synthetic CRMs are traceable to pure compounds and are shipped with certificates stating certified values and their uncertainties.
Our specialized team of CRM manufacturing experts can prepare synthetic CRMs for you based on your needs. There are 45 possible additional elements!
Examples of material that can be analyzed:
The standards are fused to remove mineralogical and particle size effects. Fused samples are ‘perfect’ samples, and in combination with the Fundamental Parameters (FP) matrix correction model enable very wide concentration ranges in a single calibration.
Fusion is ideal for accurate analysis of light elements as these are typically most affected by particle size and mineralogical effects. Find out more about sample preparation by fusion.
The standards are delivered as powders which can be prepared on-site as fused beads using the included Lithium borate flux. The Base set can be complemented with several pre-defined or bespoke extension sets.
The Base set provides 15 multi-element standards for the analysis of the 11 most common oxides in a variety of materials such as ores, minerals, slags and geological materials and is shipped with monitors and templates suitable for the Axios-mAX, Zetium or Epsilon 4 spectrometers.
Oxide Coverage and their concentration ranges (wt%): | |
---|---|
Na2O | 0-50 |
MgO | 0-80 |
Al2O3 | 0-80 |
SiO2 | 0-90 |
P2O5 | 0-50 |
SO3 | 0-59 |
K2O | 0-40 |
CaO | 0-80 |
TiO2 | 0-80 |
Mn3O4 | 0-80 |
Fe2O3 | 0-80 |
Product name | Compatibility | Part number |
---|---|---|
WROXI-CRM Base WD | Zetium, Axios-mAX | 943 0043 63011 |
WROXI-CRM Base ED | Epsilon 4 | 943 0043 63021 |
WROXI-Pro Extension is an add-on to the WROXI Base set of CRMs. This extension set provides 12 multi-element standards for the analysis of 10 additional oxides in a variety of materials such as ores, minerals, slags and geological material.
It is shipped with monitors and templates suitable for the Zetium and Axios-mAX spectrometers.
Oxide Coverage and their concentration ranges (wt%): | |
---|---|
V2O5 | 0-10 |
Cr2O3 | 0-10 |
NiO | 0-10 |
CuO | 0-10 |
ZnO | 0-10 |
SrO | 0-40 |
ZrO2 | 0-40 |
BaO | 0-40 |
HfO2 | 0-10 |
PbO | 0-10 |
Product name | Compatibility | Part number |
---|---|---|
WROXI-CRM Pro Extension for WD XRF | Zetium, Axios-mAX | 943 0043 63031 |
WROXI-CRM Cement is an extension to the WROXI Base set of CRMs. This extension set provides 9 multi-element standards for the analysis of 10 additional analytes in a variety of cements and the raw materials used in its manufacture, including limestone, clay/ shale, gypsum clinker, raw meal fly ash, slags and iron ore. It is shipped with monitors and templates suitable for the Zetium, Axios-mAx or Epsilon spectrometers.
Elemental Coverage and their concentration ranges (wt%): | |
---|---|
Al2O3 | 0-10 |
SiO2 | 0-32 |
CaO | 50-63 |
ZnO | 0-1 |
Cr2O3 | 0-1 |
Fe2O3 | 0-7 |
F | 0-1 |
Cl | 0-1 |
SrO | 0-1 |
BaO | 0-1 |
SO3 | 0-0,5 |
Product name | Compatibility | Part number |
---|---|---|
WROXI-CRM Cement Extension for WD XRF | Zetium, Axios-mAX | 9430 043 63041 |
WROXI-CRM Cement Extension for ED XRF | Epsilon 4 | 9430 043 63051 |
The traceability can be ensured all along the analytical chain by combining the data security audit trailing on our spectrometer, the sample monitoring options on our sample preparation equipment, and the CRMs produced with metrological traceability.