X-ray diffraction is the ideal tool for direct quantification of the mineralogical composition of raw materials, clinker and cement products. CubiX³ Cement features a detector designed for rapid data collection and sample measurement takes less than five minutes. Specially configured for high-throughput production and process control in cement industries, the diffractometer can be integrated in an automation setup for a variety of sample types (e.g. 40 mm or 51 mm rings) and fed by a robot or a transport belt.

Application support for turnkey cement solutions

Users have the option of tailor-made Rietveld solutions, as well as the ability to customize general solutions. Larger laboratories can also be set up to develop central solutions using the full HighScore Plus suite, which can then be deployed to a plant-wide network of CubiX3 Cement instruments. 

RoboRiet runs at the production plants. It enables the operator to run such Rietveld quantifications completely automatically and transfers the results to a customer defined destination (LIMS, paper, table…)

High-speed sample throughput featuring quick turnaround times

Ultra-fast sample loading in combination with a high-speed linear detector such as X’Celerator allow a higher sample throughput that enables the user to control their processes more effectively. Measurement times of 5 minutes can be easily achieved.

Push-button measurements for easy operation and virtually no learning curve

CubiX³ Cement makes data collection, analysis and reporting straightforward. Every step can be fully automated and Malvern Panalytical’s software range supports the specialized analytical techniques required by cement producers. Specific industry regulation compliance is built in.

CubiX³ Cement building materials analysis uses Malvern Panalytical’s Industry software that includes classical phase quantification such as free lime analysis.

Robust design for industrial environments

The robust design of the CubiX³ Cement allows the use of the X-ray diffractometer even in remote and dusty locations. The goniometer, optics and detectors are dust protected inside the enclosure to prevent unexpected downtimes.

GeneralOpticsSample handling
Goniometer: θ-θ for completely horizontal sample handlingCu tubeProgrammable spinner
Diffractometer: 200 mm radiusFixed and programmable divergence and anti-scatter slits availableUltra-fast pneumatic loader
Software: Industry, HighScore Plus, optional with Walk-up packageSecondary monochromator for Cu64 position X’Changer with 2 x 30 positions plus 4 preferred loading positions
X’Celerator detector (RTMS)X’Handler for belt connection with 2 additional positions
Automation possible with any automated laboratory

CubiX³ Cement

Detectors

X'Celerator

Image

The world’s first 1D silicon strip detector for laboratory X-rays

As the world’s first silicon-based position-sensitive 1D detector for XRD, the X’Celerator is the result of the pioneering development from Malvern Panalytical. With the R&D 100 Award-winning X’Celerator detector you can perform XRD measurements up to 100 times faster than with a traditional point detector, without compromising data quality. With no need for cooling water, liquid nitrogen flow, counting gas or time-consuming calibrations, it is a cost-effective solution.

The X’Celerator is designed exclusively for Malvern Panalytical’s diffractometers for applications in research and industry.

One solution for multiple materials

Push-button analysis of:  

Portland cement clinker, Portland cement (CEM I), gypsum raw material, limestone, fly ash, blast furnace slag, aluminate cement, blended cements (CEM II CEM III CEM IV CEM V) and any other materials upon request.

Sample preparation of clinker

Application Note

Knowledge center

Want access to free online webinars, white papers, user manuals and much more?

View resources