The RImax is a modular system consisting of the GPCmax integrated solvent and sample delivery module, refractive index detector, column oven, plus the same powerful OmniSEC software used in the TDAmax research system.

  • Relative molecular weight measurement and molecular weight distribution of polymers and proteins
  • Autosampler incorporated to increase throughput and improve repeatability
  • In line degasser and automatic eluent sensor for out of solvent warning
  • Column oven to give repeatable elution profiles
  • Advanced GPC/SEC software capable of going from data to results in just two clicks
  • Upgradable to add light scattering (RALS and LALS) intrinsic viscosity and UV detectors, to provide absolute molecular weight, molecular size, structure and composition of proteins and polymers

The GPCmax contains an integrated pump, autosampler and degasser. Mobile phase, stored in solvent bottles placed on top of the instrument, enters the dual piston pump after passing through the eluent sensor. This will automatically stop the flow if the solvent is exhausted mid-run. An inline degasser then removes dissolved gases from the mobile phase, which improves the baseline on any of the detectors that may be connected. The pump is compatible with any solvent, even acidic buffers.

The autosampler inside the GPCmax can hold up to 120 vials, which can either be heated, or cooled to prevent degradation of the samples over time. The Autosampler provides the system with variable, reliable, accurate and reproducible injection volumes, enabling comprehensive macromolecular characterizations to be made with confidence.

Mobile phase (and sample) passes through the GPC/SEC chromatography columns in the column oven. After eluting from the column, the dissolved polymer molecules are now separated by size and pass through the RI detector before going to waste.

A complete GPC/SEC system to provide a conventional, calibration system for relative molecular weight measurement.

Output of Mn, Mw, Mz, Mp, Mw/Mn, dn/dc, Weight Fraction (IV [η], Rh, Rg, Branching Number, Branching Frequency, Concentration, MH-a, MH-k, A2, dA/dc all optional)

Component 1

System:
GPCmax
Pump flow rate:
0.01 to 9.99 mL/min, programmable soft start
Pulsation:
Less than 1%, measured with viscometer
Degasser:
Two channels, < 0.5ppm oxygen at 0.5mL/min, eluent sensor to stop pump when eluent runs out
Dimensions (W, D, H):
55cm x 38cm x 53cm
Weight:
37kg

Component 2

System:
Autosampler
Capacity:
120 vials, programmable sequence
Injection volume:
Variable 20 to 150µL
Reproducibility:
Better than 0.5%
Carryover:
Less than 0.1%, depending on wash program
Cooling option:
4°C to 40°C, limited to 60 vials
Heated tray option:
Up to 65°C limited to 60 vials heated, 60 vials unheated

Component 3

System:
Refractive index detector
Measurement principle:
Deflection
Light source:
Tungsten lamp
Cell volume:
9µL
Purging:
Manual, automatic and programmable
Data acquisition rate:
2Hz to OmniSEC
Temperature control range:
35° - 55°C in 1°C steps – normal environment
10° - 30°C in 1°C steps – cold room environment
Dimensions (W, D, H):
220mm x 350mm x 160mm
Weight:
12kg

Detector (option)

Detector:
UV, Single wavelength programmable
Wavelength:
190 to 500nm
Light source:
Deuterium
Cell volume:
10µL
Data acquisition rate:
Analog, A-to-D with 5Hz to OmniSEC

Column Oven

Temperature control range:
10°C above ambient to 100°C
Capacity:
Up to five 8mm x 30cm GPC columns
Internal dimensions (W x H x D):
7cm x 4cm x 41cm

General

Laser safety:
Class 1
Software:
OmniSEC, 6 channels at 5Hz, unlimited acquisition time

Operating environment

Temperature:
15°C – 40°C
Humidity:
35% - 80% non-condensing

Viscotek RImax

Viscotek GPCmax

Image

Integrated Pump, Autosampler and Degasser, perfect for size exclusion and gel permeation chromatography.

The GPCmax is a solvent and sample delivery module exclusively for GPC/SEC applications. It provides the reliable and stable chromatographic foundation for the Viscotek advanced detection systems.

More information

Viscotek UV Detector

Image

Concentration detector, perfect for GPC/SEC, molecular weight determination and compositional analysis.

Accurate measurement of the polymer or protein concentration profile is essential to good molecular weight or structure data. The high-stability Viscotek UV detector is ideally suited for multi-detection GPC/SEC.

More information

Viscotek RI Detector (VE3580)

Image

High-stability concentration detector, perfect for GPC/SEC chromatography and molecular weight determination.

Accurate measurement of the polymer or protein concentration profile is essential to good molecular weight or structure data. The high-stability Viscotek RI is ideally suited for multi-detection GPC/SEC.

More information

OmniSEC software

Image

Powerful, agile, easy to use GPC/SEC software for instrument control, data acquisition, analysis and reporting.

OmniSEC software is an integrated solution for the advanced analysis of proteins and polymers by GPC/SEC, and is at the heart of all Viscotek systems and detectors. Selectable "protein" or "polymer" user interfaces with simplified work flows improve productivity and help you to maximize the information and efficiency of your experiments. Simply load your samples and the software controls all the sequencing, enabling truly automatic unattended operation.

More information

GPC and SEC Columns

Image

GPC/SEC columns for all aqueous and organic applications

A wide range of columns for analytical GPC/SEC of synthetic and natural polymers and proteins.

More information

Viscotek GPC/SEC Heated Column Oven

Image

Modular chromatography ovens for holding columns up to 100°C or 150°C

The Viscotek GPC Heated Column Ovens are modular chromatography ovens for holding columns at temperatures from ambient up to 100°C or 150°C

More information

GPC and SEC Standards

Image

A range of molecular weight standards for different applications of GPC/SEC

Malvern Panalytical offers a wide range of molecular weight standards for GPC/SEC for conventional and universal calibration as well as light scattering.

More information

Protect your investment and ensure optimized performance at all times with Malvern Panalytical's service plans.

When you purchase a Malvern Panalytical product we understand that this is just the first stage of a working relationship that will last for the lifetime of the instrument. Depending on your needs, Malvern Panalytical will provide the support for your business.

Help Desk

Training

Software downloads

Malvern Panalytical's service options- choose the right plan for you:

Malvern Panalytical Platinum Plan

For laboratories where maximizing instrument up-time is critical to its daily performance. Our highest level of response and the 'all inclusive' price plan takes care of those unexpected repair bills should the unfortunate occur.

Malvern Panalytical Gold Plan

Enhance your laboratory productivity by maintaining instrument efficiency. Still receive that priority response, combined with specialist technical and software support, we'll keep your instrument performance on track to deliver.

Malvern Panalytical Bronze Visit

For laboratories looking to optimize instrument performance, regular preventative maintenance is essential.

Platinum PlanGold PlanBronze Visit
Annual PM/PV Test
yes
yes
no
Telephone / Email Support
yes
yes
no
Priority Response
yes
yes
no
Emergency Breakdown visits*
yes
yes
no
Parts Included
yes
no
no
Technical & Software Support
yes
yes
yes
IQ/OQ (Pharma)***
yes
yes
yes

*including labour & travel costs***available at an additional cost