Designed for unprecedented analytical accuracy and repeatability, Claisse® electric and gas automatic instruments set new benchmarks in fusion capabilities. The same is true for Claisse pre-fused and homogeneous borate fluxes, high-quality platinumware, as well as analytical consulting services. A wide range of Consumables is also available. 

Supported products

Claisse Eagon 2

Safe, simple, high performance
Image
Measurement
Elemental analysis
Number of samples per fusion cycle
2
Productivity
Glass disks (XRF) : up to 8 per hour
Heating mode
Electric
Technology
Borate fusion

Claisse TheOx Advanced

Get ready for high productivity!
Image
Measurement
Elemental analysis
Number of samples per fusion cycle
6
Productivity
Glass disks (XRF): up to 24 per hour; Borate and peroxide solutions (ICP-AA): up to 36 per hour
Heating mode
Electric
Technology
Borate fusion

Claisse rFusion

Let the Claisse rFusion work for you
Image
Measurement
Elemental analysis
Number of samples per fusion cycle
6
Productivity
Glass disks (XRF): up to 24 per hour; Borate solutions (ICP-AA): up to 48 per hour
Heating mode
Gas
Technology
Borate fusion

Claisse M4

The standard in sample preparation by fusion
Image
Measurement
Elemental analysis
Number of samples per fusion cycle
3
Productivity
Glass disks (XRF): up to 12 per hour; Borate solutions (ICP-AA): up to 24 per hour
Heating mode
Gas
Technology
Borate fusion

Claisse LeNeo

Keeping ahead through Claisse expertise in fusion
Image
Measurement
Elemental analysis
Number of samples per fusion cycle
1
Productivity
Glass disks (XRF) : up to 4 per hour; Borate and peroxide solutions (ICP-AA): up to 6 per hour
Heating mode
Electric
Technology
Borate fusion

Claisse LeDoser

Scale up your analytical precision
Image
Measurement
3D structure / imaging
Precision
Up to 0.0001g
Productivity
Runs autonomously for up to 250 weighings (depending on quantity of flux)
Technology
Borate fusion

Claisse LeDoser-12

Just-in-time weighing for optimal precision and repeatability!
Image
Measurement
3D structure / imaging
Productivity
Runs autonomously for up to 250 weighings (depending on quantity of flux)
Technology
Borate fusion