Advanced Triple Detection GPC of High Molecular Weight Polyacrylamide Resin

Polyacrylamide resins have traditionally been difficult to analyze by conventional chromatographic methods due to their high polarity, structural inconsistencies, and hydrogen bonding capabilities. A specialized method has been developed