Nylon 6,6 vs. 6,12:Adapting Chromatographic Methods to Subtle Structural Differences

A chromatographic study of Nylon 6,6 and Nylon 6,12 illustrates how small changes in the chemical structure of a polymer can provide an opportunity to optimize chromatographic parameters