Cement is a composite material which may contain more than 20 components. Use of Morphologically-Directed Raman Spectroscopy (MDRS®) available on the Malvern Panalytical Morphologi® ID system enables the individual components to be characterized for particle size and particle shape. Increased understanding of the particulate composition of cements is vital for reduction of production costs and the optimization of cement blends.