This application note demonstrates the performance of the Axios FAST XRF spectrometer for the analysis of low alloy steel.

Accurate and fast elemental analysis during the production process of steel and its base materials is a critical requirement. Measurements were performed using an Axios FAST simultaneous X-ray fluorescence spectrometer equipped with a 4 kW Rh SST-mAX X-ray tube. 