Zetium - Analysis of iron ores using the WROXI widerange oxides application

This data sheet demonstrates the performance of the Zetium - Minerals edition XRFspectrometer in providing accurate and precise iron ore analyses.

Iron ores typically consist of oxides of iron together with gangue minerals like silica, bauxite, alumino-silicates and phosphorous bearing apatite. In addition to the iron ore grade, these gangue minerals influence the price of the iron ore since they affect the smelting process and the quality of the iron and steel.