NTA: Principles and Methodology

The need to characterize different properties of nanomaterials continues to grow rapidly. Since the commercialization of the technique in 2004, Nanoparticle tracking Analysis (NTA) has become increasingly prevalent in a wide variety of different research fields and industrial applications. In this introductory chapter of the Nanoparticle Tracking Analysis (NTA) application and usage review, we discuss the principles and methodology of the technique including sizing, concentration measurement and fluorescence detection.  