A drilling mud, or drilling fluid, is an oil or water-based mix of minerals (barite, calcium carbonate), salts and polymers formulated to protect the drill and the shaft during oil or gas production.

Analysis of drilling muds and drilling mud constituents is necessary to understand, monitor and control:

  • Molecular weight distributions and structure of polymer additives for a resource-efficient product
  • Particle size distribution and shape consistency to prevent aggregates that might cause damage, prevent the escape of gas and block pores
  • Zeta potential – to manage salt concentration and minimize aggregate formation from the outset.

Malvern Panalytical offers laboratory solutions used in studying the parameters influencing formulation and composition and manufacture on-line particle sizing solutions for in-use monitoring of drilling muds.

Linha Mastersizer

Linha Mastersizer

Os analisadores de tamanho de partículas mais utilizados no mundo.

Mais detalhes
Medição Tamanho da partícula
Faixa de tamanho das partículas: 0.01µm - 3500µm
Tecnologia Difração laser
Tipo de dispersão Via úmida, A seco, Via úmida e a Seco

OMNISEC

OMNISEC

O sistema GPC/SEC com vários detectores mais avançado

Mais detalhes
Medição Estrutura molecular, Tamanho molecular, Massa molecular, Viscosidade, Agregação de proteínas
Faixa para peso molecular 200Da - 10MDa
Massa de amostra mínima (polistireno) 100ng
Massa de amostra mínima (BSA) 100ng
Tecnologia Cromatografia de permeação em gel, Cromatografia por Exclusão de Tamanho (SEC), Espalhamento de luz estático

The petro edition of Zetium

The petro edition of Zetium

The new element in petrochemicals

Mais detalhes
Medição 3D structure / imaging
Precisão 1% (sem condensação)
Tecnologia X-ray Fluorescence (XRF)

Epsilon 1 para óleos lubrificantes

Epsilon 1 para óleos lubrificantes

Simplificando a análise de aditivos em óleos lubrificantes

Mais detalhes
Medição Elemental analysis, Contaminant detection and analysis, Elemental quantification
Gama elementar Na-Am
Resolução (Mg-Ka) 145eV
LLD 1 ppm - 100%
processamento de amostra 40per 8h day - 80per 8h day
Tecnologia X-ray Fluorescence (XRF), Energy Dispersive X-ray Fluorescence (EDXRF)

Linha Mastersizer

Linha Mastersizer

Os analisadores de tamanho de partículas mais utilizados no mundo.

OMNISEC

OMNISEC

O sistema GPC/SEC com vários detectores mais avançado

The petro edition of Zetium

The petro edition of Zetium

The new element in petrochemicals

Epsilon 1 para óleos lubrificantes

Epsilon 1 para óleos lubrificantes

Simplificando a análise de aditivos em óleos lubrificantes

Mais detalhes Mais detalhes Mais detalhes Mais detalhes
Medição Tamanho da partícula Estrutura molecular, Tamanho molecular, Massa molecular, Viscosidade, Agregação de proteínas 3D structure / imaging Elemental analysis, Contaminant detection and analysis, Elemental quantification
Faixa de tamanho das partículas: 0.01µm - 3500µm      
Faixa para peso molecular   200Da - 10MDa    
Massa de amostra mínima (polistireno)   100ng    
Massa de amostra mínima (BSA)   100ng    
Precisão     1% (sem condensação)  
Gama elementar       Na-Am
Resolução (Mg-Ka)       145eV
LLD       1 ppm - 100%
processamento de amostra       40per 8h day - 80per 8h day
Tecnologia Difração laser Cromatografia de permeação em gel, Cromatografia por Exclusão de Tamanho (SEC), Espalhamento de luz estático X-ray Fluorescence (XRF) X-ray Fluorescence (XRF), Energy Dispersive X-ray Fluorescence (EDXRF)
Tipo de dispersão Via úmida, A seco, Via úmida e a Seco      

Linha Mastersizer

OMNISEC

The petro edition of Zetium

Epsilon 1 para óleos lubrificantes

Linha Mastersizer OMNISEC The petro edition of Zetium Epsilon 1 para óleos lubrificantes

Os analisadores de tamanho de partículas mais utilizados no mundo.

O sistema GPC/SEC com vários detectores mais avançado

The new element in petrochemicals

Simplificando a análise de aditivos em óleos lubrificantes

Mais detalhes Mais detalhes Mais detalhes Mais detalhes
Tecnologia
Difração laser
Cromatografia de permeação em gel
Cromatografia por Exclusão de Tamanho (SEC)
Espalhamento de luz
Espalhamento de luz estático
Energy Dispersive X-ray Fluorescence (EDXRF)
Wavelength Dispersive X-ray Fluorescence (WDXRF)
X-ray Fluorescence (XRF)