Characterizing Li-ion Battery Separators: Pore Structure Determination

Faça login para assistir a este webinar

Esqueci minha senha
Ainda não está cadastrado? Criar uma conta

Lithium-ion (Li-ion) batteries are an advanced technology that will play a key role in the trend toward renewable and sustainable industrial electrification solutions.

The AutoPore V Series utilizes the Mercury Porosimetry analysis technique, based on the intrusion of mercury into a porous structure under stringently controlled pressures. Besides offering speed, accuracy, and a wide measurement range, mercury porosimetry permits you to calculate numerous sample properties such as pore size distributions, total pore volume, total pore surface area, median pore diameter and sample densities (bulk and skeletal). This webinar will describe how the AutoPore V can be used to characterized separators which are critical to the safety and reliability of li-on batteries.

Palestrante

  • Jeff Hrivnak - Vice President of Market Development, Micromeritics
  • Tony Thornton - Senior Product Scientist Director, Product Integrity and Performance, Micromeritics