Catalyst active site insight, without waiting for beamtime

Portrait beside illustrated catalyst pellets and molecular structures on a dark blue background.
Jan Gertenbach explores how laboratory XAS brings insight into catalyst oxidation state and local atomic structure into routine research.

A catalyst’s long-range crystalline structure may remain similar as it moves from fresh to activated and eventually deactivated, even while the chemistry around the active metal changes. Spotting those changes has usually meant competing for limited synchrotron beamtime to access X-ray absorption spectroscopy (XAS), so these measurements happen rarely rather than routinely.

That’s the predicament Dr. Jan Gertenbach addressed at our Future Days: Catalysts event on September 22, while stepping in for his colleague Dr. Hadeel Hussain. Jan has spent his career studying how structure shapes material behavior, from crystal engineering of porous gas-storage materials at Stellenbosch University to 12 years as an XRD specialist at Malvern Panalytical. Today, he is one of our Market Development Managers.

His session, ‘Seeing the active site: bringing electronic-structure and local-environment insight into the everyday catalyst laboratory,’ showed how laboratory XAS brings oxidation state and local coordination into routine catalyst development. Here’s a recap of his insights.

Catch up on the full session and more from Future Days: Catalysts.

What changes around the active atom

As a catalyst is activated and later deactivates, its average crystal structure can remain similar, while the oxidation state, coordination, and bond distances around the active metal change. XRD reveals the broader structure; XAS reveals the electronic state and local environment of a selected element. As Jan put it, the key question is what changes around the active atom, and how we can study it to understand how a catalyst works.

XAS answers that question through two regions of the spectrum. The X-ray absorption near edge structure (XANES) reveals the element’s oxidation state, electronic structure, and local geometry. Meanwhile, the extended X-ray absorption fine structure (EXAFS) shows its neighboring atoms, coordination number, and bond distances. Because XAS is element-specific and doesn’t depend on long-range crystallinity, it can probe active sites that XRD alone can’t fully describe, providing an additional perspective on the material and how it works.

Bringing XAS into the lab

Jan was clear that laboratory XAS complements synchrotrons rather than replacing them. Synchrotrons remain essential for frontier experiments, very dilute systems, rapid time resolution, and specialized environments.

A laboratory source is less intense, so measurements can take hours rather than seconds. What it offers instead is cadence. Researchers can screen more samples, repeat measurements when their questions change, and measure references alongside unknowns. They can also arrive at the synchrotron with better-prepared, more focused experiments.

On Empyrean XAS, Malvern Panalytical’s multipurpose diffractometer, XAS runs alongside XRD on a single instrument.

From static samples to changing conditions

Jan demonstrated the approach on Cu-BTC, a copper-based metal-organic framework, measured alongside copper foil and copper oxide references

The XANES edge position was much closer to the CuO reference than the copper foil reference, indicating that the copper oxidation state is closer to +2 than 0, while EXAFS gave a first-shell Cu-O distance of 1.938 Å and a coordination number of four.

Jan sees two developments shaping future workflows:

Automated sample changing could make it faster and more efficient to move between materials with less manual intervention.

Non-ambient environments add controlled temperature and atmosphere, so activation and redox treatments can be studied as they happen. Laboratory XAS brings the active-site view into the routine development loop: formulate, measure, understand, and improve. Jan described XAS as “an added arrow to our quiver,” one that leads to earlier decisions and helps researchers choose their next experiment faster.

Key questions from the Q&A

What essential equipment would you recommend for a startup working on sustainable aviation fuel synthesis with the Fischer-Tropsch process?

“Everything, of course,” Jan joked. In practice, he said, a startup may not need its own instruments at first, since running costs can be prohibitive, and service laboratories can support it through the early stages. He suggested an elemental analyzer and particle sizing as starting points, though qualifying a product for sale soon calls for a much broader range of techniques. The panel’s advice was to team up with bigger players.

How do analytics and metrology tie into catalysis?

Materials science is a circular science, Jan explained: you formulate, make a material, then measure it to understand its properties and behavior. Each measurement is a decision point before the next step, so it has to be accurate, reproducible, and done in a standard way the whole community agrees on.

Watch the recording of this session to see how lab XAS tracked nickel’s oxidation state inside a charging battery, and more from Future Days: Catalysts.