Today’s waste is tomorrow’s feedstock. Catalysis makes it possible.

Every year, billions of tons of CO2, agricultural residues, and plastic waste leave the economy with valuable carbon and hydrogen still locked inside. The right catalyst can bring that value back.
This is what Ignacio Garcia highlighted at our Future Days: Catalysts event on September 22. Ignacio is General Manager for PID Eng&Tech at Malvern Panalytical. Ignacio started his career as a chemical engineering researcher and has spent the past 17 years developing, commercializing, and deploying chemical reactor technologies at PID Eng&Tech.
At Future Days: Catalysts, Ignacio presented ‘From waste to value: catalysis for a more circular industry.’ During his talk, he explained why circularity matters, explored the catalytic routes that turn CO2 and biomass into fuels and chemicals, and set out what it will take to design the next generation of catalysts. Here’s a recap of his insights.
Catch up on the full session and more from Future Days: Catalysts.
Why a circular industry needs catalysis
As the world’s population grows and industry scales up worldwide, global energy demand keeps climbing. Echoing Maurits van Tol’s opening talk, Ignacio noted that nobody wants to go back to lower living standards – so we must instead find ways to make the resources we already have go further.
Industry has long run on a linear model: extract resources, convert them into products, and dispose of what’s left. Each year, an estimated 37 billion tons of CO2 are emitted into the atmosphere, alongside around 5 billion tons of agricultural biomass residues, plus food waste, industrial off-gases, and plastic waste. All still contain valuable carbon and hydrogen that could be put back to work.
A circular model brings those molecules back into the economy. Catalysis makes that practical by making waste conversion efficient, selective, less energy-intensive, and economically viable.
From waste streams to fuels and chemicals
Ignacio illustrated this conversion opportunity with two of the largest waste streams: CO2 and biomass. The key conversion steps on these routes rely on catalysts for speed and efficiency.
- Converting CO2 to methanol: Hydrogenating waste CO2 over copper–zinc oxide catalysts produces methanol, a marine fuel and platform molecule that can become formaldehyde, olefins for plastics, gasoline, or sustainable aviation fuel (SAF).
- Biomass gasification to fuel: Gasification turns biomass into syngas, a mixture of hydrogen and carbon monoxide. Fischer-Tropsch synthesis then converts that syngas into hydrocarbons for gasoline, SAF, and plastics.
- Biomass pyrolysis to fuel: Heating biomass in an inert atmosphere yields bio-oil, char, and gas. Upgrading the bio-oil by hydrodeoxygenation (HDO) produces hydrocarbons that can also become gasoline or SAF.
Proving that a promising route can work industrially takes evidence at every stage, Ignacio explained, from characterization techniques such as hydrogen temperature-programmed reduction (H2-TPR) to catalyst testing and scale-up in pilot units.
Catalyst characterization comes first
The core scientific challenge is striking the right balance between activity, selectivity, and stability. Activity drives conversion rates and lowers capital costs, selectivity maximizes the target product, and stability determines catalyst lifetime and industrial reliability. Getting all three right is especially hard with highly stable molecules like CO₂ and complex, oxygen-rich biomass compounds.
That means answering four questions, each supported by different characterization techniques:
- Where is the active site? Identifying the active site is the first step toward rational catalyst design. Chemisorption quantifies metal surface area and dispersion, while lab-based X-ray absorption spectroscopy (XAS) reveals the active metal’s oxidation state and local coordination.
- How does structure drive performance? Small structural changes can dramatically influence activity and selectivity. Gas adsorption and mercury intrusion porosimetry map pore structure, while XRD identifies crystalline phases and crystallite size.
- Why does the catalyst deactivate? Coke formation, sintering, poisoning, and structural changes all shorten catalyst lifetime, and improving lifetime is often as important as improving activity. Raman spectroscopy, XRD, and XRF can help reveal the cause.
- What does the data tell us? Combining in-situ characterization, big data, machine learning, and multiscale modeling moves catalyst development away from trial and error, toward knowledge-driven design.
What the next generation of catalysis looks like
Ignacio identified four developments that will shape the catalysts of the future:
- Advanced materials, including single-atom, nanostructured, and multifunctional catalysts that can carry out complex conversions in a single step.
- Operando and in-situ characterization, moving beyond composition analysis to track how a catalyst changes in real time under reaction conditions, and how that affects performance.
- AI-driven catalyst development, using machine learning to predict catalyst behavior and guide synthesis, with experimental validation to confirm the results.
- Digitalization and automation, from automated reactor labs and high-throughput experimentation to digital twins, speeding up catalyst screening and validation.
As Ignacio concluded, the stakes are high. Catalysis will influence how many resources we consume, and how much value we recover from the waste we produce. The better our understanding of catalysts, the better we can design waste-to-value catalysts with the optimal balance between activity, selectivity, and stability – and the faster we can achieve a more circular future.
Key questions from the Q&A
Are operando measurements harder to run and interpret?
Yes, Ignacio agreed, and that’s part of the challenge. The aim is to understand what’s happening in the catalyst’s structure in real time, under the conditions an industrial process actually operates at.
What does operando analysis mean for catalyst manufacturers?
Operando analysis could help catalyst manufacturers better understand how catalysts change under reaction conditions and how those changes affect performance. As Ketjen’s Matthew Rayner explained, hydroprocessing catalysts, for example, only become active after treatment in the reactor. The opportunity is to develop measurement setups that more closely reproduce industrial pressures and temperatures, allowing researchers to study catalysts in their working state.
Watch the recording of this session to find out more about how operando techniques, AI, and automation will speed up catalyst design, and learn more from Future Days: Catalysts.
{{ product.product_name }}
{{ product.product_strapline }}
{{ product.product_lede }}