With the latest innovations in X-ray tube and detector technology in the Epsilon 4, this system, in combination with the Eagon 2 fully automatic fusion system, complies with the latest cement testing methods of both ASTM C114-15 and ISO 29581-2.

The data presented in this datasheet clearly demonstrate the compliance of the Epsilon 4 XRF spectrometer, in combination with the Eagon 2 automatic fusion machine, with both the ASTM C114- 15 and ISO 29581-2:2010 cement test methods in 10 minutes for the quantitative analysis of SiO2, Al2O3, Fe2O3, CaO, MgO, SO3, K2O, Na2O, TiO2, P2O5, ZnO and Mn2O3 in cement, prepared as fused beads.