A degas study was conducted to determine the effectiveness of flow versus vacuum degas. An amorphous silica-alumina and a microporous zeolite were prepared by both techniques and then nitrogen isotherms were collected for both materials. The resulting isotherms established equivalence between vacuum versus flow degas.
A degas study was conducted to determine the effectiveness of flow versus vacuum degas. An amorphous silica-alumina and a microporous zeolite were prepared by both techniques and then nitrogen isotherms were collected for both materials. The resulting isotherms established equivalence between vacuum versus flow degas.