Using Multi-Detection GPC/SEC to Determine Impact of Sterilization on Medical-Grade Polymers

This article gives an introduction to multi-detection GPC/SEC and presents data that shows how the technique is being used to determine the impact of sterilization on medical grade poly(L-lactide).

This article gives an introduction to multi-detection GPC/SEC and presents data that shows how the technique is being used to determine the impact of sterilization on medical grade poly(L-lactide).