Lubrication oils: wear metal analysis

Turnkey solution for accurate analysis of wear metals in lubrication oils

The appearance of wear metals in lubricating oils is a significant indicator of component wear or contamination. Accurate XRF analysis of trace elements in oil, and monitoring their levels over time, helps optimize preventive maintenance programs. The data can be used for an early detection of potentially expensive failures, this way reducing repair costs and increasing safety margins.

Expertise program for XRF analysis of wear metals in lubrication oils

The following elements and concentration ranges are covered by the Wear Metals Expertise program:

Elements ppm Elements ppm
Ag 0 - 500 Mo 0 - 500
Al 0 - 2000 Na 0 - 500
Ba 0 - 2000 Ni 0 - 500
Ca 0 - 5000 P 0 - 2000
Cd 0 - 500 Pb 0 - 500
Cr 0 - 500 Sb 0 - 500
Cu 0 - 400 S 0 - 500
Fe 0 - 500 Sn 0 - 500
K 0 - 500 Ti 0 - 500
Mg 0 - 3000 V 0 - 500
Mn 0 - 500 Zn 0 - 2000

In addition to standards, the program includes a complete methodology, from sample preparation to quality assurance, to be used with Malvern Panalytical’s XRF systems.

Included:

  • Suite of calibration standards as required for the norm(s) including validation sample
  • P-1 or P-2 cups and assembly tool and pre-cut Mylar foils, sufficient for calibration and validation
  • Setup of optimized analysis program and system calibration, enabling best throughput and accurate results, allowing routine analysis by factory operators
  • Setup of methodology validation and calibration maintenance procedure
  • Advice on sample preparation best practices workflow optimization
  • User training and documentation

Optional

  • Statistical Process Control  for setting up QA/QC workflows*
  • Integration of the Wear Metal method into your standard operating procedures, including documentation and deployment at one or multiple sites

Prerequisites

  • Malvern Panalytical XRF spectrometer: Zetium, Axios or MagiX WD XRF systems, equipped to run liquid samples, or an Epsilon 3 or higher range system
  • Oil-Trace  module for SuperQ or Epsilon software, which corrects for variations in the oxygen to hydrocarbon ratio of samples, allowing best accuracy and use of a single calibration for multiple matrices