1. From the Applications Lab: Using GPC/SEC to Analyze Elastomers
01:38
2. Abstract and Overview
00:46
3. Outline
00:57
4. Outline
00:07
5. What are Elastomers?
00:53
6. Untitled
03:03
7. What Is Chromatography?
00:35
8. Size Exclusion Chromatography
02:35
9. The Separation Process
03:25
10. Components of a GPC/SEC System
02:14
11. Detectors for GPC/SEC Systems
02:38
12. Outline
00:19
13. Styrene-Butadiene Rubber (SBR) Data
00:42
14. GPC Analysis of SBR
01:48
15. GPC Analysis of SBR
00:23
16. Numerical Data for Samples A & B
01:22
17. Branching Analysis of SBR
01:53
18. Branching Analysis of SBR
01:10
19. Flow Injection Polymer Analysis (FIPA)
01:21
20. FIPA of SBR
00:41
21. Numerical Data from FIPA of SBR
00:30
22. Difference between FIPA and GPC Analysis
02:59
23. Butyl Rubber Data
00:49
24. GPC Analysis of Butyl Rubber
00:45
25. GPC Analysis of Butyl Rubber
00:25
26. Numerical Data for Samples A & B
01:54
27. Mark-Houwink Plot of Butyl Rubber
00:43
28. Conclusions
01:12