This data sheet shows that Epsilon 3XLE is very capable of analyzing low levels of Cr, Ni, Cu, Zn, As, Br, Cd, Ba, Hg and Pb in polyethylene samples.

In collaboration with DSM-Resolve a set of standard reference materials was developed for the analysis of catalysts residues and potentially toxic elements in polyethylene (TOXEL). 