Using transmission XRD in Aeris to measure the crystalline to amorphous ratio in polymers

IntroductionPolymer solids can have a range of mechanical properties, at one extreme they can be very soft and elastic and at the other they can be immensely strong and rigid. Their mechanical properties can change with external conditions such as temperature and pressure. They can be used for a large range of applications from protective coatings to containers and building materials. The ...