| 00:00:00 | Laser Diffraction for Battery Manufacturing |
| 00:00:57 | Laser Diffraction for Battery Manufacturing Presented by Joe Wolfgang, Diffraction Product Manager, North America |
| 00:02:37 | Laser Diffraction Reasons for success….. |
| 00:03:51 | Mastersizer 2000 Advanced measurements made simple… |
| 00:04:57 | What does Laser Diffraction measure? |
| 00:05:34 | Huygen Diffraction from a single droplet |
| 00:05:58 | What does Laser Diffraction Measure? Changes in light scattering as a function of particle/droplet size |
| 00:07:25 | Scattering data analysis… Mie Theory |
| 00:08:55 | A basic laser diffraction system… |
| 00:09:42 | Mastersizer 2000 Optical Design Red Light Scattering |
| 00:10:23 | A typical laser diffraction data set… Coarse Particles |
| 00:10:53 | A typical laser diffraction data set … Sub-Micron Particles |
| 00:11:06 | Scattering data analysis… |
| 00:11:56 | What is particle size? |
| 00:13:16 | Ceramics: Agglomerate detection… |
| 00:14:08 | Latex standard measurements… |
| 00:14:43 | You are not just buying a Malvern product….you are investing in Malvern |
| 00:15:17 | Modern Battery Construction |
| 00:15:59 | What is so important about Lithium? |
| 00:16:20 | Charging & Discharging |
| 00:16:59 | A Li-ion battery is an electromechanical device which converts stored chemical energy directly into electricity |
| 00:17:26 | The energy path |
| 00:18:16 | The internal structure of the electrode plays an important part in the performance of the battery |
| 00:19:48 | Some electrode properties of interest include |
| 00:20:40 | The internal structure of the electrode plays an important role in the performance of the battery |
| 00:21:23 | Real Powder particles |
| 00:21:41 | Thanks to |
| 00:22:42 | Contact Information |
This recorded webinar explores why laser diffraction is useful for particle size and size distribution measurements during the the manufacture of today's state-of-the-art batteries.