Analysis of Cd, Sn, Sb, Cs, Ba, La, Le and Nd in rocks and soils - improved detection limits using K-series lines

Detection limits for typical medium-power wavelengthdispersive spectrometers (WDXRF) configured for geological applications are illustrated in this application note.

A series of soil and rock standards were used to calibrate the application. The soil samples were analyzed in the form of pressed powder pellets