Analysis of rawmix samples- simple sample preparation, quick analysis, accurate and precise result

This application note shows that the Epsilon 3XLE is capable of analyzing major and minor compounds like Na2O, MgO, Al2O3, SiO2, SO3, K2O, CaO, TiO2 and Fe2O3 in rawmix samples prepared as pressed powders.

In the cement industry the composition of the input material plays a very important role in the production process and in the quality of the end product. XRF analysis is a useful tool for controlling the composition of the raw material.