| 00:00:00 | Laser Diffraction Masterclass 6 – Troubleshooting: What to do when things go wrong |
| 00:01:01 | A six part series with 1 through 4 now available on-demand |
| 00:01:40 | Laser Diffraction Masterclass 6 – Troubleshooting: What to do when things go wrong |
| 00:02:20 | The laser diffraction masterclass 2019 |
| 00:03:26 | Masterclass 6 - Troubleshooting |
| 00:04:20 | Common questions from laser diffraction users |
| 00:06:08 | Data Quality: How to Tell If the System is Clean |
| 00:06:08 | Data Quality: How to tell if the system is clean |
| 00:06:08 | Data Quality: Poor backgrounds |
| 00:07:25 | How to Clean the Wet Cell Windows |
| 00:07:25 | Data Quality: Poor Backgrounds |
| 00:07:25 | Data Quality: Poor Backgrounds |
| 00:07:25 | Use the software to help |
| 00:08:49 | Why do I see unexpected modes in my results? |
| 00:10:02 | Unexpected large particles |
| 00:10:56 | Unexpected large particles |
| 00:12:12 | Hydro Sight |
| 00:12:47 | Anomaly detection |
| 00:13:43 | Unexpected large particles |
| 00:14:08 | Unexpected large particles |
| 00:14:39 | Unexpected large particles |
| 00:15:26 | Why do I see unexpected modes in my result? |
| 00:16:46 | What causes high residuals? |
| 00:18:16 | How much sample should I add? |
| 00:19:31 | How much sample should I add? |
| 00:20:58 | How much sample should I add? |
| 00:21:58 | Why are my results not stable? |
| 00:23:36 | Why are my results not stable? |
| 00:24:20 | Why are my results not stable? |
| 00:25:17 | Why are my results not stable? |
| 00:25:48 | Why are my results not stable? |
| 00:27:37 | Why are my results not stable |
| 00:28:11 | Why are my results not stable |
| 00:28:22 | Why are my results not stable |
| 00:29:17 | What affects measurement reproducibility? |
| 00:30:56 | Checking the performance of your system |
| 00:32:17 | Common questions from laser diffraction users |
| 00:33:26 | Q&A |
| 00:41:25 | A six part series with 1 through 4 now available on-demand |
However good the methods we develop are, there is still the potential for something to go wrong! In this webinar we will cover what you can do if you are presented with results that are not what you expect. We will show you how to review measurement data to determine if the measurements have been carried out correctly, and to recognise common errors. If you have any specific issue that you would like us to cover, please email your questions before the presentation date.
Présentateur
Anne Virden Ph.D. - Technical Support Supervisor Analytical Laser Diffraction
Pour en savoir plus
Who should attend?
Anyone who makes laser diffraction measurements!
Anyone who reviews particle size data from a laser diffraction instrument
Anyone with questions about laser diffraction measurements
Why attend?
To learn what to do if your particle sizing results aren’t what you expect
To learn how to assess data quality in laser diffraction measurements