This webinar presents a generalized approach to modeling the pore size distribution which has been developed to determine the complete distribution of macro-, meso-, and micro-pores.

Rather than using a fragmented approach of simple overlays from individual techniques, the Unified Method provides a full pore size distribution and improved estimate of total pore volume of the material. The resulting pore size distribution has the benefit of simultaneously predicting both the adsorption (or desorption) isotherm and the mercury intrusion porosimetry.