Automating cement analysis

Reviewing a decade of online particle sizing

Oliver Schmitt, Malvern Instruments UK, and Thomas Schuster, Zementwerk Berlin, Germany, dscuss the crucual role of online analysis in the manufacture of slag cement.
In 2014, Zementwerk Berlin GmbH & Co. KG installed a new online particle size analyzer on one of its two grinding circuits, replacing an initial unit commissioned more than 10 years ago. This article will review what has been achieved over the intervening decade and discuss how online analysis has proven instrumental in enabling the manufacture of slag cement.