Investigating the Molecular Weight and Structure of Linear and Cross-Linked Hyaluronic Acid by SEC-MALS and SEC-Triple Detection

This article demonstrates the application of a multi-angle light scattering (MALS) detector within a triple detector array to measure absolute molecular weight distribution and gain insight into molecular structure for an application involving the analysis of hyaluronic acid.

This article demonstrates the application of a multi-angle light scattering (MALS) detector within a triple detector array to measure absolute molecular weight distribution and gain insight into molecular structure for an application involving the analysis of hyaluronic acid.