| 00:00:00 | Elemental analysis of a wide range of oxides: A new approach |
| 00:00:59 | Poll Questions |
| 00:00:59 | Elemental analysis of a wide range of oxides: A new approach |
| 00:01:24 | Poll Answers |
| 00:01:24 | WROXI: Wide range oxides |
| 00:01:54 | Challenge: elemental analysis of diverse materials |
| 00:03:26 | Outline |
| 00:03:58 | What is WROXI? |
| 00:05:25 | Which elements and concentration ranges? |
| 00:07:19 | Elemental analysis of minerals by XRF |
| 00:10:14 | Fused bead method |
| 00:11:50 | Why fuse |
| 00:13:20 | Why WROXI? |
| 00:14:56 | Calibration strategy in XRF |
| 00:15:55 | Calibration strategy in XRF |
| 00:17:20 | How to implement WROXI |
| 00:19:03 | How to set it up |
| 00:19:08 | Measure and Calibrate in the usual way |
| 00:20:13 | WROXI – Application notes |
| 00:21:04 | WROXI – validation of accuracy |
| 00:22:22 | WROXI – accuracy (1 of 2) |
| 00:22:47 | WROXI – accuracy (2 of 2) |
| 00:22:59 | Comments |
| 00:25:23 | XRF technologies |
| 00:27:27 | XRF technologies |
| 00:28:33 | Examples of ED and WD calibrations |
| 00:29:08 | Can pressed powders be used with WROXI |
| 00:31:09 | Pressed powder in-house standards procedure |
| 00:32:13 | WROXI – key benefits |
| 00:33:49 | Thank you for attendingLive Q & A session & On demand Q & A sessionemail to:events@malvernpanalytical.com |
When daily operations require elemental analysis of a wide range of inorganic/geological samples, it is often cumbersome, or not possible to set up and maintain a large number of dedicated calibrations to handle such range. In these cases, a widely applicable, but accurate solution is highly desirable. In this webinar, we demonstrate Malvern Panalytical's unique solution WROXI in combination with Epsilon 4, which is capable to handle a wide range of sample types.
Key topics include:
-
Elemental analysis
of minerals by XRF
- WROXI – validation of accuracy
-
XRF technologies
- Examples of ED and WD calibrations
- WROXI – key benefits