Physical adsorption is a technique used to characterize the surface and pore features of solids, that is, the materials texture. 

The adsorption isotherm generated by the Physical Adsorption technique enables one to characterize a solids' texture by determining its surface area, porosity, and total pore volume.

This webinar is the third part of a three part series.