This data sheet describes the benefits of resolving the mineralogical ore composition by use of X-ray diffraction (XRD) in order to optimize operational efficiency of the mining and beneficiation process of Sn-W-Nb ore.

Knowing the qualitative and quantitative mineral composition of Sn-W-Nb ore gives additional information for downstream processing. Using a benchtop diffractometer in a laboratory or in automation helps to frequently monitor ore mineralogy and allow immediate decision making to achieve optimal efficiency during mining and beneficiation. 