Six zeolite samples were analyzed simultaneously using the ASAP 2420 equipped with the Micropore option. This option enables you to perform micropore analyses on all six ports at the same time, comparable to the High Throughput mode. These analyses were performed using argon as the adsorptive at 87K. Typical micropore analyses using nitrogen may take as long as five to seven days. By using argon, the analyses can be shortened to as little as two days.
Six zeolite samples were analyzed simultaneously using the ASAP 2420 equipped with the Micropore option. This option enables you to perform micropore analyses on all six ports at the same time, comparable to the High Throughput mode. These analyses were performed using argon as the adsorptive at 87K. Typical micropore analyses using nitrogen may take as long as five to seven days. By using argon, the analyses can be shortened to as little as two days.
Please download to read more.