This verification sample can be used to ensure your Grazing Incidence Small Angle Scattering (GISAXS) setup works correctly. The sample consists of spherical Fe2O3 nanoparticles with a known size distribution, attached to the surface of a Si wafer. The particles have a polystyrene shell.


The specifications of the particles are certified by SEM and GISAXS analysis.