This data sheet shows that the Epsilon 3X – a high-performance energy dispersive X-ray fluorescence spectrometer – is capable of analyzing Mn, Fe, Mg, Al, Si, P, S, K, Ca, Sr and Ba in manganese ore samples.

Manganese ore is an important raw material for metal industries. Manganese is a key component of stainless steel formulations and widely used aluminum alloys. Accurate elemental analysis of manganese ore samples play a very important role in manganese ore mine mapping. The concentrations of Mn and Fe determine manganese ore pricing. The presence of P and S has strong influence on the quality of steels and aluminum alloys. XRF analysis is a useful tool in classifying and controlling the compositions of the manganese ore materials. 

Login

Not registered yet?

Sign up for free today. By registering you will have free access to exclusive content including

  • Webinars, presentations and videos
  • Application notes, technical notes, articles, white papers and software downloads

And in addition you will receive

  • Our regular eNews including the latest news, education, events and offers from Malvern Panalytical