This application note describes a straightforward, robust method for the analysis of RoHS elements in polyethylene, being representative of many polyolefins types, according to F2617.

XRF has emerged as an optimal solution for the screening of toxic heavy metals regulated by the EU Directives, RoHS (Restriction of Hazardous Substances), WEEE (Waste Electronic and Electrical Equipment) and ELV (End of Life, Vehicles). 