Analysis of boron in glass using a PX7 multi-layer crystal

This application note demonstrates the capability of the Ultimate edition of the Zetium XRF spectrometer for the analysis of B2O3 in glass. The system has the precision, accuracy and repeatability required for the fast and reliable analysis of B2O3 in glass samples.

The worldwide production of glass today can be divided into three main types of product: borosilicate glass, soda-lime glass and lead glass. These different types of glasses have different chemical and physical properties and are produced by accurately adjusting the chemical composition by the fine balance of the different raw materials. 