BET specific surface area by static gas adsorption
Brunauer-Emmett-Teller (BET) specific surface area (SSA) by static gas adsorption Certified Reference Materials (CRM) kits from Micromeritics offer a convenient method for confirming the operation of your system, providing peace of mind for the verification and monitoring of your instrument’s performance.
Brunauer-Emmett-Teller (BET) specific surface area (SSA) by static gas adsorption technique.
Standards: ISO 9277, USP846, ASTM C1069
Instruments: TriStar, 3Flex, ASAP 2020, ASAP 2460, ASAP 2425, Gemini
| Part Number | Material |
|---|---|
| 004-16880-00 | Alumina 5m2/g, 6 vials |
| 004-16881-00 | Alumina 1m2/g, 6 vials |
| 004-16882-00 | Alumina 185m2/g, 6 vials |
| 004-16884-00 | Alumina 28m2/g, 6 vials |