Date recorded: November 26 2019

Duration: 26 minutes 11 seconds

Sand is mostly used as a raw material in the production of many industrial products such as glass and cement, while aluminosilicates are used in the building, refractory and catalyst industry. It is important to know the exact compound concentrations of these materials so they remain within the tolerances over time,  contribute to cost savings and avoid waste. This project demonstrates that the use of borate fusion with Claisse LeDoser and LeNeo instruments are highly efficient in the preparation of sand and aluminosilicate samples for the analysis with an XRF spectrometer. You will discover that it is fast, easy and efficient. Borate fusion is an excellent alternative to other sample preparation techniques in the laboratory.

Table of contents
1. Keys to Successful Analysis - Borate Fusion of Sand & Aluminosilicates
00:17
2. Introduction
01:58
3. Overview
00:34
4. Sand & Aluminosilicates
02:00
5. Sand & Aluminosilicates
01:48
6. Purpose of the Project
00:32
7. Fusion Method and Instrumentation
00:08
8. Sand & Aluminosilicates
00:51
9. Sand & Aluminosilicates
02:18
10. Sand & Aluminosilicates
00:53
11. Equipment Used
00:36
12. LeNeo
00:49
13. LeDoser
03:16
14. Borate flux
00:28
15. Fusion Methodology
00:58
16. Fusion Methodology– Glass industry
00:39
17. Calibration Strategy and Selection of Control Sample
00:09
18. Calibration Strategy
01:13
19. Final Results
00:08
20. Evaluation of Performance
00:53
21. Evaluation of Performance
00:47
22. Conclusion
00:34
23. Questions and Thank You!
04:22