| 00:00:00 | Polymer molecular size - the original nanoparticles |
| 00:01:32 | Polymer solution characterization - Part 2. Polymer molecular size - the original nanoparticles? |
| 00:01:58 | Polymer molecular size - the original nanoparticles? |
| 00:02:28 | Polymer is a composite of the Greek words poly and meros, meaning “many parts.” |
| 00:03:38 | The importance of molecular size in solution |
| 00:06:54 | Molecular weight vs. Molecular size |
| 00:09:05 | Static light scattering vs. Dynamic light scattering |
| 00:12:20 | DLS Instrument Components |
| 00:13:08 | Intensity Fluctuations and Brownian Motion |
| 00:13:44 | Correlation in Dynamic Light Scattering |
| 00:14:06 | Correlation in Dynamic Light Scattering |
| 00:14:24 | Correlation: Small Particles, Rapid Fluctuations |
| 00:14:32 | Correlation:Small Particles, Rapid Fluctuations |
| 00:14:43 | Correlation:Small Particles, Rapid Fluctuations |
| 00:15:04 | Correlation:Small Particles, Rapid Fluctuations |
| 00:15:11 | Correlation:Small Particles, Rapid Fluctuations |
| 00:15:13 | Correlation:Small Particles, Rapid Fluctuations |
| 00:15:23 | Correlation Functions |
| 00:16:07 | Correlation Functions |
| 00:16:47 | DLS measurement of polystyrene in toluene |
| 00:17:42 | Batch Mw measurement |
| 00:19:17 | Static Light Scattering |
| 00:20:46 | MALS |
| 00:23:24 | Molecular weight and size using MALS |
| 00:24:47 | Molecular weight and size by MALS |
| 00:26:08 | Angular dependence in PS235k |
| 00:26:30 | Molecular Size Determination from GPC/SEC measurements. |
| 00:26:53 | Molecular size |
| 00:28:21 | BSA |
| 00:28:43 | BSA |
| 00:30:44 | Complex polysaccharide |
| 00:31:07 | Complex polysaccharide |
| 00:34:09 | Determining molecular size - summary |
| 00:35:25 | For more information …… |
| 00:35:59 | Molecular size |
| 00:42:37 | Contact Information |
Long before 'nanoparticle' became a common term, polymer scientists were already working at the nano scale (<100nm) with polymer macromolecules. Determining the accurate size at that scale is a challenge and often different applications will require different technical solutions. In the second webinar in this series, we will look at measurement of polymer molecular size in solution. The focus is on light scattering techniques including DLS and MALS.