Smart and Programmable Sponges from Design and Synthesis to Implementation

Log in to watch this webinar

Not registered yet? Create an account

Join our guest speaker Dr Omar Farha, Associate Professor of Chemistry at Northwestern University, where he will focus on metal–organic frameworks (MOFs) from basic research to implementation and commercialization. MOFs are a class of porous, crystalline materials composed of metal-based nodes and organic ligands that self-assemble into multi-dimensional lattices. In contrast to conventional porous materials such as zeolites and activated carbon, an abundantly diverse set of molecular building blocks allows for the realization of MOFs with a broad range of properties. We have developed an extensive understanding of how the physical architecture and chemical properties of MOFs affect material performance in applications such as catalytic activity for chemical warfare agent detoxification.

Speakers

  • Dr. Omar K. Farha - Professor Of Chemistry, Northwestern University