DLS in 30 Minutes – Q&A
A webinar entitled “DLS in 30 Minutes” was given in June which attracted a very large audience. The presentation introduced dynamic light scattering and covered the principles of the technique, a discussion of how the measurement is performed, how the data is analyzed and how the results obtained should be interpreted.
We were inundated with various questions during the webinar and we only had time to answer a few on the day. The remainder of questions were answered via e-mail but we thought it would be good to share some of these in this blog.
If you missed the webinar, you can view a recording on our website.
DLS measures the random motion of particles undergoing Brownian motion and the technique will not be applicable when the particle motion is not random. Therefore, the upper size limit is sample dependent and is normally defined by either the onset of particle sedimentation or by number fluctuations.
All particles will sediment and the rate will depend upon the particle size and relative densities of the particles and suspending medium. For successful DLS measurements, the rate of sedimentation should be much slower than the rate of diffusion since a consequence of slow diffusion is long measurement times.
The presence of sedimentation can be determined by checking the stability of the count rate from repeat measurements of the same sample. Count rates which are decreasing with successive measurements indicates that sedimentation is present and the Expert Advice system will highlight this to the user.
Another factor that needs to be considered when the sample contains large particles will be the number of particles present in the measurement volume. The measurement volume is the intersection of the laser beam and detector optics.
The intensity of scattered light produced by large particles would be sufficient to make successful measurements. However, the number of particles in the measurement volume may be so few that severe fluctuations of the momentary number of particles in the scattering volume will occur. This phenomenon is known as number fluctuations and results in large fluctuations in the scattered intensity which masks those due to Brownian motion.
The presence of number fluctuations is observed as elevated baselines and/or increases in the correlation curve, examples of which are shown below. For a random process, such as Brownian motion, the correlation curve should always decay.

When the fluctuations are large, the intercept will vary and may be greater than 1 as shown in the right-hand correlation function. This may make the result unreliable. In this case, it is recommended that the large particles are removed by filtration or centrifugation or allowed to naturally sediment over an extended period.
The maximum size we have measured is 10 microns (9 microns peak mode) which was a sample of polystyrene latex prepared in 13% w/v sucrose to density match the particles.
A measured intercept value of greater than 1 normally means that the sample contains very large particles/aggregates/dust which are causing an interference with the measurements. We refer to these as number fluctuations (please see question above).
When a sample exhibits this type of correlation function, then it is not suitable for DLS and that the large material must be removed before the measurements are retaken.
Blue pigments are challenging with a red laser. However, with a NIBS instrument (i.e. backscatter 173° detection angle), if the sample is strongly absorbing the laser, the measurement position will automatically move towards the cuvette wall. There are, therefore, no precautions to take as such. Simply try to measure the sample and see how good the intercept is in the correlation function. If the measured intercept is less than 0.1, the sample should be diluted and re-measured confirming that the size obtained is independent of the sample concentration [ISO22412 (2017)].
The following link is to an application note which details measurements made on concentrated blue pigments using a Nano S NIBS instrument.
Monitoring pigment milling processes using Dynamic Light Scattering
The lower size limit of DLS depends on many factors such as the optical configuration of the instrument, laser wavelength/power, detector sensitivity, sample concentration and excess level of scattering. This latter point is the difference in scattering between the dispersant used and the molecule/particles in the dispersant. The greater the level of excess scattering, the easier it is to measure.
The smallest size measured on a Zetasizer is 0.6nm (peak mode) and here is a technical note detailing the measurements.
Zetasizer Nano S and ZS Specifications DLS Minimum Size Limit
Most sizing techniques use an equivalent spherical diameter because the size of a sphere can be described with a single number i.e. the diameter or radius. All particle size analysis techniques measure some property of a particle and report results as the equivalent spherical diameter based on this measured parameter. Therefore, different measurement techniques often give different sizes for the same sample.
For non-spherical particles, DLS will give the diameter (or radius) of a sphere which has the same average translational diffusion coefficient as the particles being measured.
The easiest way to detect whether sedimentation is present in your sample is to take several repeat measurements (say 3 or 5) and look at the mean count rates from each of the measurements. If sedimentation is present, the mean count rate will decrease each time the sample is measured. Here is an example of some results obtained for a sample containing sedimenting particles………..
If the mean count rate decreases between repeat measurements, the sample will be changing each time it is measured. Correlation functions from repeat measurements should perfectly overlap with each other such as these…………
However, if sedimentation is present (or the sample is changing with time), then the correlation functions from repeat measurements will not overlap with each other. For example………….
Please also note that the baselines of the correlation functions are elevated (i.e. they are not flat). This is evidence of number fluctuations which are defined as variations in the number of particles within the scattering volume during a DLS measurement as further discussed above.
Related Content:
- Zetasizer Nano S and ZS Specifications DLS Minimum Size Limit (Technical note)
- Application of DLS to Protein Therapeutic Formulations: Principles, Measurements and Analysis – 1. Basic Principles
- An Introduction to DLS Microrheology
{{ product.product_name }}
{{ product.product_strapline }}
{{ product.product_lede }}