Zetasizer Nano Series

The new Zetasizer Nano series allows the measurement of the three most important parameters for the analysis of colloids and polymer compounds: particle size, zeta potential, and molecular weight. These instruments incorporate new technology that offers exceptional sensitivity and a wide range of functionalities. Malvern’s patented NIBS light technology is applied to the Nano Z and Nano ZS, allowing samples to be measured without dilution or with slight dilution. The Zetasizer Nano ZS is the top instrument in Malvern’s Zetasizer Nano series, capable of measuring all three parameters without performance adjustment.

The Nano ZS, Z, and ZS90 instruments all use Malvern Instrument’s proprietary disposable zeta potential cell, preventing contamination between samples.

 

     * Particle Size – NIBS technique can measure the size of particles and molecules in the range of 0.3nm to 10µm.

 

     * Zeta Potential – M3-PALS technology can accurately measure the zeta potential of samples in both aqueous and non-aqueous dispersants.

     * Molecular Weight – Using an Avalanche Photodiode detector and fiber optic transmission devices provides the sensitivity and stability required for absolute molecular weight measurement.

 

▶ Product Specifications

  1. Common Specifications

     * Temperature range: 0°C – 90°C

     * Condensation air: Purge equipment using dry air/nitrogen
     * Laser: 4mW He-Ne, 633nm
     * Laser attenuator: Automatic, transmitted from 100% to 0.0003%
     * Detector: Avalanche Photodiode, Q.E: over 50% at 633nm
     * Laser class: Class 1 conforming to EN 60825-1:2001 and CDRH
     * Size: 320mm, 600mm, 260mm(W,D,H)
     * Weight: 21kg

 

  2. By Parameter

   ** Size Measurement

 

 Nano ZS

Nano S 

Nano Z 

Nano ZS90 

Nano S90 

 Particle Size Range

(Diameter)

 0.3nm ~ 10µm

0.3nm ~ 10µm

 

 0.3nm ~ 5µm

0.3nm ~ 5µm 

 Minimum

Sample Volume

12µl

12µl 

 

20µl

20µl

 Minimum

SampleConcentration

0.1mg/mL Lysozyme 

0.1mg/mL Lysozyme 

 

 

 

 Maximum

SampleConcentration

 40%w/v

40%w/v 

 

 

 

 

  ** Zeta Potential Measurement

 

Nano ZS

Nano S 

Nano Z 

Nano ZS90 

Nano S90 

 Particle Size Range

(Diameter)

3.8nm – 100µm

 

3.8nm – 100µm

3.8nm – 100µm

 

 Zeta Potential

Range

No practical limit

 

No practical limit

No practical limit 

 

 Electrophoretic

Range

No practical upper limit

 

No practical upper limit

No practical upper limit

 

 Conductivity Range

0 to 200mS/cm

 

0 to 200mS/cm

0 to 200mS/cm

 

 Sample Concentration

Range

Up to 40%w/v

 

Up to 40%w/v

Up to 40%w/v

 

 

  ** Molecular Weight Measurement

 

Nano ZS

Nano S 

Nano Z 

Nano ZS90 

Nano S90 

 Absolute Molecular Weight Range

(Debye Plot)

980Da – 2×107Da

980Da – 2×107Da

 

9,800Da – 2×107 Da

9,800Da – 2×107Da

 Molecular Weight Range

(Mathematical Diameter)

342Da – 2×107Da

342Da – 2×107Da

 

342Da – 2×107Da

342Da – 2×107Da