This white paper examines the impact of particle properties on suspension viscosity, and more broadly on rheological behavior. It looks in some detail at how particle size, shape and zeta potential influence critical aspects of suspension performance such as viscosity and stability and how these properties can be manipulated to tailor rheological behavior.