Selecting the most stable biotherapeutic antibody using Differential Scanning Calorimetry

Stability is a crucial issue for the development of therapeutic antibodies and genetically tailored antibody fragments. Poor stability may affect antibody expression levels in various cell types, result in fractional populations of non-functional or misfolded material, or lead to the formation of large and potentially immunogenic protein aggregates over time.

Antibodies and antibody-like proteins represent a large and growing number of molecular entities entering human clinical trials in virtually all disease indications. Antibodies are heterotetramers composed of heavy and light chains. Constant domains (CH and CL chains) contain invariable amino acid sequences which depend upon the antibody isotype and subclass. In contrast, antibody variable domains are extraordinarily diverse, enabling the recognition of virtually any foreign antigen with high specificity and affinity. Variable domain diversity is derived by the pairing of variable heavy (VH) and variable light (VL, kappa or lambda) chains, numerous linker sequences between variable and constant domains, and hypersomatic mutation. Diversity within variable domains may also lead to stability variations from one antibody to another.

Until recently, there has been a relative paucity of stability data regarding full-length antibodies, potentially due to the fact that they are complicated, multi-domain proteins. Here, we investigated the domain-dependent unfolding properties of 17 human or humanized IgG1 and IgG4 antibodies using Differential Scanning Calorimetry DSC (1). These included Tysabri™ (clinically approved for the treatment of multiple sclerosis), seven molecules in phase I or II trials, four molecules on track for investigational new drug (IND) filing with the FDA in 2007, and six molecules in research. The dataset can be used as a reference guide to help researchers in the field of antibody discovery understand whether thermal stability may be an issue for any given antibody molecule.

The second part of this application note describes a process to engineer stability back into a particularly unstable antibody. A combination of stabilizing mutations resulted in a Fab with a midpoint of thermal unfolding (Tm) of 92°C measured by DSC. Stabilization resulted in greatly enhanced functional expression of the antibody fragment in E. coli (2).

Introduction

Stability is a crucial issue for the development of therapeutic antibodies and genetically tailored antibody fragments. Poor stability may affect antibody expression levels in various cell types, result in fractional populations of non-functional or misfolded material, or lead to the formation of large and potentially immunogenic protein aggregates over time.

Antibodies and antibody-like proteins represent a large and growing number of molecular entities entering human clinical trials in virtually all disease indications. Antibodies are heterotetramers composed of heavy and light chains. Constant domains (CH and CL chains) contain invariable amino acid sequences which depend upon the antibody isotype and subclass. In contrast, antibody variable domains are extraordinarily diverse, enabling the recognition of virtually any foreign antigen with high specificity and affinity. Variable domain diversity is derived by the pairing of variable heavy (VH) and variable light (VL, kappa or lambda) chains, numerous linker sequences between variable and constant domains, and hypersomatic mutation. Diversity within variable domains may also lead to stability variations from one antibody to another.

Until recently, there has been a relative paucity of stability data regarding full-length antibodies, potentially due to the fact that they are complicated, multi-domain proteins. Here, we investigated the domain-dependent unfolding properties of 17 human or humanized IgG1 and IgG4 antibodies using Differential Scanning Calorimetry DSC (1). These included Tysabri™ (clinically approved for the treatment of multiple sclerosis), seven molecules in phase I or II trials, four molecules on track for investigational new drug (IND) filing with the FDA in 2007, and six molecules in research. The dataset can be used as a reference guide to help researchers in the field of antibody discovery understand whether thermal stability may be an issue for any given antibody molecule.

The second part of this application note describes a process to engineer stability back into a particularly unstable antibody. A combination of stabilizing mutations resulted in a Fab with a midpoint of thermal unfolding (Tm) of 92°C measured by DSC. Stabilization resulted in greatly enhanced functional expression of the antibody fragment in E. coli (2).

Materials and methods

Materials and methods used in these studies were described previously (1,2). DSC work was performed using a Malvern MicroCal VP-Capillary DSC system. The current Malvern Panalytical  MicroCal PEAQ-DSC systems are improved on sample consumption (smaller capillary cell volumes) and feature a single, user friendly control and data processing software.  

[MRK2053-01_fig01a] 636217451192369007DF.png

[MRK2053-01_fig01b] 636217451434235662QI.png

Fig 1. (A) DSC curve of the BIIB7 IgG1. Above the curves are structures of a full-length human IgG1 antibody (13). (B) DSC curves representing the four human IgG subclasses. Reprinted from (1) with the permission of Elsevier.

[MRK2053-01_fig02a] 636217451704226315TO.png

[MRK2053-01_fig02b] 636217451946092969WH.png

Fig 2. (A) DSC thermal unfolding curves of four human or humanized IgG1 antibodies, BIIB16, BIIB6, BIIB4, and BIIB1. (B) DSC unfolding curves of the BIIB7 antibody in both the IgG1 and IgG4 formats. Reprinted from (1) with the permission of Elsevier.

Fab stability measurements of 18 human or humanized IgG sequences

Since their constant domains are virtually identical, IgGs of similar subclass vary in stability based on differences in their Fv regions. To investigate the range of IgG Fab stabilities that exist for human or humanized antibodies, particularly IgG1s, DSC studies were performed using a panel of 18 full-length human(ized) antibodies, denoted BIIB1–18. The Fab transitions generally had CPmax values (i.e., the height of a DSC peak) approximately three-fold greater than that of the CH2 or CH3 domains as shown by the DSC trace of BIIB7 (Fig 1A). Characteristic DSC traces of the four human IgG subclasses are shown in Figure 1B with IgG1 demonstrating the highest apparent antibody Fc stability. Aggregation during the unfolding process affects Fab Tm measured by DSC (3,4); therefore, each DSC scan was performed under identical conditions for each antibody, and the information obtained was considered a relative measure of each domain’s stability.

BIIB1-18 Fab transitions varied significantly in their relative thermal stability as a result of differences in their Fv regions. The DSC curves shown in Figure 2A illustrate how individual Fv regions can lead to different Fab unfolding behaviors. The range of Fab Tm values for the 18 BIIB antibodies was 57.2 °C to 81.6 °C (Table 1). The three antibodies with the lowest Fab Tm values, BIIB15-17, demonstrated multiple unfolding transitions for their Fabs suggesting a breakdown in the cooperativity of unfolding (see Fig 2A for BIIB16’s DSC curve). The Fab peak for these antibodies was split into two transitions. The transitions with the lower T are listed in Table 1. A second transition, which may represent the unfolding of CH1/CL, occurred with Tm values of 74 °C, 72 °C, and 70 °C for BIIB15, BIIB16, and BIIB17, respectively.

Table 1: BIIB IgG Fab Tm values from DSC
IgGFab Tm (°C)VH sub-classVK sub-class
BIIB181.6VH1VK1
BIIB278.5VH1VK1
BIIB378.2VH1VK2
BIIB477.7VH3VK2
BIIB577.1VH4VK1
BIIB676.8VH3VK1
BIIB775.9VH1VK3
BIIB875.6VH1VK1
BIIB974.7VH3VK4
BIIB1074.7VH4VK1
BIIB1173.1VH1VK4
BIIB1271.2VH1VK4
BIIB1370.8VH3VK4
BIIB1470.6VH7VK-†
BIIB1568.5VH3VK1
BIIB1668.0VH3VK3
BIIB1757.2VH3VK2
BIIB18-*VH3VK2
* Did not express
† Unusual kappa, germline undetermined.
Reprinted from (1) with the permission of Elsevier.

Although the DSC studies were performed with ideal heterotetrameric proteins as determined by size-exclusion chromatography, the antibody with the least stable Fab, BIIB17, expressed poorly and accumulated high molecular weight aggregates if left in solution at 2 °C to 8 °C for over 1 week. The CH2 and CH3 unfolding transitions of each IgG1 superimposed well (representative DSC traces shown in Fig 2A). The same was true for the CH2 and CH3 transitions of the three IgG4s (data not shown).

BIIB7 was constructed as both an IgG1 and IgG4. IgG1 and IgG4 CH1 sequences have ten amino acid differences (six are conservative) and a different disulfide-bonding pattern with CL. The apparent Fab Tm values of BIIB7 in the IgG1 and IgG4 format were similar (ΔTm < 1°C, Fig 2B) after deconvolution of the peaks. This similarity suggests that Fab thermostabilities between IgG1 and IgG4 can be directly compared.

Engineering Fab residues to improve stability

It is well-established that proteins can be stabilized with consensus design – the mutation of rare amino acids to the consensus amino acids found in homologous protein sequences. In support of this, the humanized BIIB antibodies with the poorest stability as determined by DSC, appeared to have the greatest levels of uncommon amino acid types in their frameworks. In an effort to develop antibody and antibody fragment stabilization strategies, we selected a poorly-behaved Fab, and performed a mutagenesis campaign to engineer stability back into the Fab. We began with a Fab that recognized tetanus toxoid (αTT) and was derived from a human source (5). We chose 45 residue positions for randomization. Full details on this saturation mutagenesis campaign are described in (2).

[MRK2053-01_fig03] 636217452186553427PZ.png

Fig 3. DSC analysis of the wild-type αTT Fab and all 12 Fabs containing various mutant combinations including V11, the most stable Fab. The identity of each curve can be derived based on the ΔTm listed in Table 2. Reprinted from (2) with the permission of Oxford University Press.

Table 2. Thermostabilizing mutations led to highly stable Fab variants with increased bacterial expression and apparent functionality
FabHC MutantsLC MutantsΔTm* (DSC)Δexpress†ΔMidpoint‡ (μg/ml)
WT--0.01.0±0.463.0
V1V1 V11L, S77T, F89I-5.02.325.0
V2V11L, S77T, T72N, A84L, F89I, G118AD9L, N22S, W50A, N152G7.92.08.9
V3S77T, T72N, A84L, F89I, G118AD9L, N22S, W50A7.83.83.5
V4V11L, S77T, F89IN22S, W50A5.33.226.0
V5V11L, S77T, F89TN22S, W50A3.92.650.0
V6V11L, S77T, F89IN22S, W50H6.71.713.0
V7S77T, G127AD9L ,N22S, W50A2.41.925.0
V8V11L, S77T, T72N, A84P, F89I, G118AD9L, N22S, W50A, N152G8.93.910.0
V9V11L, S77T, F89TW50A4.33.520.0
V10V11L, S77T, T72N, A84P, F89I, G118AD9L, W50A, N152G9.73.37.1
V11V11L, S77T, T72N, A84P, F89I, G118A, G24AD9L, N22S, W50H, N152G13.33.0±0.34.0
V12V11L, S77T, T72N, A84P, F89I, G118AD9L, W50H, N152G11.12.62.8
* WT Tm = 78.7°C, scan rate = 1.0°C/min
† E. coli expression level normalized to 1.0 for the WT αTT Fab whose average expressed yield over three separate cultures was 0.56 ± 0.20 mg/l culture. The standard error is also
provided for V11 which was expressed twice.
‡ Fab concentration at the midpoint of the ELISA saturation curve for biotinylated tetanus toxoid. Reprinted from (2) with the permission of Oxford University Press.

Mutagenesis and thermotolerance screening of the αTT Fab library

The 45 mutant PCR reactions were individually transformed, and close to 4500 individual colonies were picked and cultured in 96-well plates containing expression media. Supernatants containing Fab were heat challenged at three separate temperatures; 70 °C, 72 °C, and 74 °C (2). Variants that demonstrated enhanced thermostability were resubjected in duplicate to the thermotolerance screen to confirm their properties.

A complete list of stabilizing mutations is provided in (2). Approximately 1 % of the variants in the library exhibited enhanced thermostability. Fourteen of the “hits” were located in the VH domain, and the remaining four in the VL domain. This result suggests the stability of the native Fab was limited by the marginal stability of the VH. Surprisingly, no mutant within the ~2000 member constant domain library was found to stabilize the Fab as a whole. We speculate that stabilizing mutations within the constant domains really do occur, but that the limited stability of the VH domain controls the temperature at which the Fab unfolds and denied our ability to observe such events, see DSC experiments below.

Another explanation for the inability to discover stabilizing mutations within the CL/CH1 region may be that the 10 minute unfolding period at elevated temperatures was not sufficient for fully unfolding the constant domains. Röthlisberger and coworkers found that unfolding of the CL/CH1 heterodimer is extremely slow (6) and that the stability of all four Fab domains benefit from this kinetic stabilization. It is possible therefore that the constant domains may not unfold during the relatively short period of the thermochallenge.

While many of the stabilizing VH mutations did not match the overall consensus, the majority of the mutations did match the consensus for at least one or more of the other VH germline subclasses (2). For example, position 72 within the αTT VH was optimized by mutation to Asn. Its consensus residue in all germline VH subfamilies is the isosteric amino acid Asp. After sequencing the library plate for residue 72, it was discovered that Asp was serendipitously not represented. Also, even though V89 is the overwhelming consensus in most human VH subfamilies, mutation to Val did not improve Fab stability. The isosteric VH2 consensus residue Thr was highly stabilizing in the screen (ΔTm > 2 °C). The similarly beta-branched Ile was one of the most stabilizing mutations discovered in the screen and is found only occasionally at this position in human VH sequences but is not the consensus residue for any VH subclass.

Four stabilizing mutants were discovered within the αTT VL domain. Mutation of the VK4 consensus residue W50 to Ala (the consensus residue for VK1) or His was highly stabilizing. Histidine is rarely found at position 50 in human kappa variable domains but is often found in human lambda variable domains. This residue is close to the VH/VL domain interface. We hypothesized that its contribution to Fab stability might be linked to potential buttressing of the VH domain since the VH domain in particular appears to limit the stability of the αTT Fab (2). However, studies with the isolated VL domain suggest otherwise (data not shown). 

Mutation from Tyr to His at this position has been reported to improve the apparent stability and expression of a scFv lacking a disulfide (7). Thus, it appears that large aromatic groups at residue 50, the most C-terminal residue of VL framework 2, were not favorable for Fv stability in multiple cases.

Results of the combination of stabilizing mutations with the αTT Fab

Twelve constructs were generated containing between three and eleven stabilizing mutations identified in the initial screen (Table 2). Various combinations were derived rationally to determine the apparent contribution each mutant provides toward Fab stabilization.

Interestingly, introduction of multiple stabilizing mutations to the αTT Fab increased Fab expression in a parallel transformation/expression experiment. The best constructs consistently exhibited >three-fold increases in expressed yield over wild-type (Table 2). The stability of each Fab was evaluated by DSC (Fig 3) and circular dichroism (CD) (data not shown). DSC and CD scans were universally irreversible and the solutions were highly turbid after heating. Due to the aggregation of the Fabs, the measured Tm values were used to rank order the apparent Fab stability.

Coupled unfolding of all four domains is a common although not universal feature of Fabs, provided they are fully disulfide-linked both intramolecularly and intermolecularly (1,3,6,8,9). Uncoupling of the unfolding reactions of multidomain proteins based on substantial differences between the intrinsic stabilities of the individual domains is not uncommon and depends on the overall affinity of the domains for one another and the total interaction surface between the domains (10,11). In the absence of any portion of the Fab, unfolding of the remaining domains may not be coupled. Rowe and Tanford have demonstrated that the VL and CL within a kappa light chain appear to denature in an uncoupled fashion when not attached to a heavy chain and instead unfold as isolated domains (12). It appears additional contacts with a heavy chain must be required for cooperativity. Röthlisberger and coworkers have recently reported exhaustive and elegant experiments demonstrating how variable domains of differing stability can unfold separately from one another while variable domains with high and similar stabilities can unite the unfolding transitions of all four domains of the Fab (6). The most stable Fab construct described here (Tm = 92 °C) appeared to be on the border of uncoupling the thermal unfolding reactions of its variable domains as well.

The thermal melting temperatures of all twelve Fab variants were used to deconvolute the individual stability contribution of each mutation. All mutations appeared to contribute additively to the stability of the Fab even though several of these residues are relatively close to one another both in primary sequence and within the tertiary fold of the Fab. The analysis indicated that four mutations account for ~86 % of the Fab stabilization. G24A, T72N, and F89I mutations within the VH domain individually increased the Tm of the Fab construct by 3.0 °C, 2.8 °C, and 2.8 °C, respectively. W50H mutation within the VL domain increased the thermostability of the Fab by 3.5 °C.

Fab thermal stability correlates with the functional protein fraction expressed by E. coli

One important consideration subsequent to framework mutagenesis was the potential effect this might have on the antigen binding function of the αTT Fab. The thermostabilizing mutations were derived from the original screen using a quantitative ELISA detecting both the CL domain and the histidine tag at the C-terminus of CH1. It has often been speculated that the dynamics of an Fv domain can have a profound effect on antigen binding. We were concerned that the stabilizing mutations introduced into the Fv framework regions may interrupt a dynamic balance important for docking the antigen.

The thermostabilizing mutations did not attenuate the function of the molecule expressed by E. coli, but in fact enhanced the apparent affinity of the αTT Fab in a functional ELISA (Table 2). Two separate wild-type Fab preparations did not titrate equally with the antigen in a functional ELISA, indicating that small variations during cell culture may subtly control the amount of functional Fab expression. Both wild-type preparations yielded less functional protein than most of the stabilized αTT Fab constructs. The functional capacity of each Fab variant appeared to be directly correlated to its stability as described by the Tm (Fig 4). As the mutations were distant from the predicted binding loops, it is unlikely that these residues directly enhance contact with the antigen.

Based on the behavior of the wild-type αTT Fab, we believe that a fraction of the Fabs secreted from E. coli are in a non-functional or misfolded form. This interpretation correlates well with the fact that the isolated VL domain, when secreted from E. coli, was in a very different conformation than the VL expressed in the oxidizing cytosolic environment of BL21trxB(DE3) (results not shown). This also explains the functional variation observed between batch productions of Fab.

[MRK2053-01_fig04] 636217452427013276AK.png

Fig 4. Plot comparing the Tm of each Fab against the midpoint concentration of each Fab’s sigmoidal functional ELISA binding curve. Reprinted from (2) with the permission of Oxford University Press.

Summary

The thermal unfolding profiles of 18 human or humanized antibodies were measured using DSC and a large range of Fab stabilities were found. Using consensus design, we performed saturation mutagenesis of a particularly unstable Fab to engineer stability. Screening of the Fab libraries using a thermochallenge assay led to the discovery of 19 stabilizing mutations within 11 sites of the Fab. Combination of stabilizing mutations led to increases in thermal stability (up to 92 °C), increased bacterial expression, and a significantly reduced level of incorrectly-folded and nonfunctional material. DSC rapidly determines the factors that contribute to antibody stability, and is a valuable stability indicating technique that can be applied throughout biotherapeutic development.

Acknowledgement

This application note was authored by Stephen J Demarest, Ellen Garber, Gang Chen, Bruce E. Kimmel, David Gustafson, Jane Wu, Jared Salbato, John Poland, Marikka Elia, Xuqiu Tan, Ken Wong, Jay M. Short, and Geneviève Hansen at Biogen Idec, San Diego, CA US.

References

  1. Garber, E., and Demarest , S.J. A broad range of Fab stabilities within a host of therapeutic IgGs. Biochem. Biophys. Res. Commun. 355, 751–757 (2007).
  2. Demarest , S. J. et al. Engineering stability into Escherichia coli secreted Fabs leads to increased functional expression. Protein Engng. Des. Select. 19, 325–336 (2006).
  3. Vermeer, A. W. P. and Norde, W. The thermal stability of immunoglobulin: unfolding and aggregation of a multi-domain protein. Biophys . J. 78, 394–404 (2000).
  4. Sánchez-Ruiz, J. et al. Differential scanning calorimetry of the irreversible thermal denaturation of thermolysin. Biochemistry 27, 1648–1652 (1988).
  5. Larrick, J. W. et al. Characterization of human hybridomas secreting antibody to tetanus toxoid. Proc . Natl. Acad. Sci. US A 80, 6376–6380 (1983).
  6. Röthlisberger, D. et al. Domain interactions in the Fab fragment: a comparative evaluation of the singlechain Fv and Fab format engineered with variable domains of different stability. J. Mol. Biol. 347, 773–789 (2005).
  7. Proba, K. et al. Antibody scFv fragments without disulfide bonds made by molecular evolution. J. Mol. Biol. 275, 245–253 (1998).
  8. Kelley, R. F. et al. Antigen binding thermodynamics and antiproliferative effects of chimeric and humanized anti-p185HER2 antibody Fab fragments. Biochemistry 31, 5434–5441 (1992).
  9. Shimba, N. et al. Comparative thermodynamic analyses of the Fv, Fab*, and Fab fragments of the anti-dansyl mouse monoclonal antibody. FEBS Lett. 360, 247–250 (1995).
  10. Ewert , S. et al. Biophysical properties of human antibody domains. J. Mol. Biol. 325, 531–553 (2003).
  11. Varea, J. et al. Structural and thermodynamic characterization of Pal, a phage natural chimeric lysin active against pneumococci. J. Biol. Chem. 279, 43679–43707 (2004).
  12. Rowe, E. S. and Tanford, C. Equilibrium and kinetics of the denaturation of a homogeneous human immunoglobulin light chain. Biochemistry 12, 4822–4827 (1973).
  13. Saphire, E. O. et al. Crystal structure of a neutralizing human IgG against HIV-1: template for vaccine design. Science 293, 1155–1159 (2001).