This application note demonstrates the capability of the Epsilon 5 energy-dispersive XRF spectrometer for performing the analysis of major and minor elements as well as selected trace elements in geological materials prepared as fused beads.

Analysis of the major element compositions of geological and industrial minerals materials are important for both geochemical research as well as industrial process control. Major and minor elements are typically measured using fused beads to expand calibration ranges and minimize matrix effects