This data sheet demonstrates that the Epsilon3XLE, a benchtop energy dispersive X-ray fluorescence spectrometer, is capable of analyzing major, minor and trace elements in soils and sediments, prepared as pressed powders.

22 compounds and trace metals are discussed: Al2O32, As, Ba, CaO, Cd, Cr, Cu, Fe2O3, K2O, MgO, MnO, Mo, Na2O, Nb, Ni, P2O5, Pb, SO, SiO2, TiO2, V and Zn. 