Laser-diffraction particle sizing pays dividends for wet-process monitoring

Sophisticated mathematics extend the range of concentrations over which measurement is feasible

In this article we take a look at how, from the starting point of an appropriate wet sensor, laser diffraction systems can be engineered to deliver to the needs of different process applications. A case study involving the control of an emulsification unit for the production of oil and water emulsions illustrates what can be achieved and the benefits delivered.

In this article we take a look at how, from the starting point of an appropriate wet sensor, laser diffraction systems can be engineered to deliver to the needs of different process applications. A case study involving the control of an emulsification unit for the production of oil and water emulsions illustrates what can be achieved and the benefits delivered.