Performing Archimedes Measurements

Resonant Mass Measurements for particle size

Brief methodology to generate a particle size distribution from the buoyant mass of particles in solution. Note the material density must be known.

Once the Archimedes has been set up, aligned, optimized and calibrated, it is ready to perform measurements. Before beginning the measurement process, ensure that the Sample port is loaded with water, the Reference port is loaded with 1/15 D2O solution and that the vials in the waste ports are empty.

Preparing the Sample

The required dilution of the sample depends on the type of sensor you are using. Exceeding these recommended dilutions increases the probability of sensor blockage and can reduce the accuracy of the concentration measurement:

    Micro H and Micro E (Up to 5 µm modal diameter, 8 µm absolute limit) – 107 particles/ml

    Nano E (Up to 1.5 µm modal diameter, 2 µm absolute limit) – 108 particles/ml

Performing a Measurement

1. Open the Experiment View on the Archimedes Software, and select “Acquire”.

2. Complete the New Experiment dialogue as per Figure 1, and click OK:

Figure 1: Experiment setup window

 Figure 1: Experiment setup window

2. When prompted, exchange the vial of water for the sample, press OK, and change the load time to 60 seconds. The resonant frequency will change as the sample loads. Press OK to cancel the load when the frequency plot plateaus. The measurement will then commence.

If the Archimedes is going to be used to carry out further measurements, it should at least be loaded with water before the next measurement to prevent cross-contamination. Ideally, the system should be cleaned as per Section 5 between measurements.

If the Archimedes is not going to be used to perform further measurements, select Load, screw vials of ethanol into the Sample and Reference ports, load the system for 60 seconds and switch off the instrument.

Customer Support

If assistance is required in the setup or use of the Archimedes, please contact your local Malvern Panalytical representative, or you can contact helpdesk

Other Basic Guides for Archimedes systems for resonance mass measurements are available:

Archimedes system setup

Archimedes sensor setup

Archimedes calibration

Cleaning your Archimedes System

Login

Not registered yet? Create an account